Material Notes:
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fiber.Vf= > 90 vol%. Tyrannohex is produced by the use of only Tyranno fiber without other matrix materials using a high-pressure machine.Very high fracture energy.Tyrannohex shows a very high fracture energy (~ 9000J/m^2) which is about 100 times as large as Si3N4 sintered body.Excellent oxidation resistance up to 1500°C in air.Almost initial strength could be maintained up to 1500°C in air. And, the initial strength was also maintained after heat-treatment at 1500°C for 1000 hours in air. (Effective formation of a protective oxide layer on the surface during early heat-treatment.)Very good creep-resistance in air compared with usual SiC/SiC composites.Difficulty of a crack formationSelf-healing eject around the interphaseDensified structureInformation provided by UBE.
Physical Properties Metric English Comments
Specific Gravity 2.54 g/cc
2.54 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 190 - 210 MPa

@Temperature 23.0 - 1500 °C
27600 - 30500 psi

@Temperature 73.4 - 2730 °F
450 - 550 MPa

@Temperature 23.0 - 1500 °C
65300 - 79800 psi

@Temperature 73.4 - 2730 °F
Modulus of Elasticity 115 GPa
16700 ksi
2D
125 GPa
18100 ksi
UD
Flexural Strength 300 - 400 MPa

@Temperature 23.0 - 1500 °C
43500 - 58000 psi

@Temperature 73.4 - 2730 °F
700 - 900 MPa

@Temperature 23.0 - 1500 °C
102000 - 131000 psi

@Temperature 73.4 - 2730 °F
Shear Strength 40.0 - 60.0 MPa
5800 - 8700 psi
2D
60.0 - 100 MPa
8700 - 14500 psi
UD
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
Fracture energy (Chevron-notch method), J/m^2
Thermal Properties Metric English Comments
Thermal Conductivity 3.90 W/m-K
27.1 BTU-in/hr-ft²-°F
2D
4.50 W/m-K
31.2 BTU-in/hr-ft²-°F
UD
Electrical Properties Metric English Comments
Electrical Resistivity 0.100 - 0.500 ohm-cm
0.100 - 0.500 ohm-cm
Specific resistance