Material Notes:
Fibermax Mat is a high-temperature, flexible mat product that is lightweight (1.5 lb/ft3 density) and highly resilient. It is composed entirely of Fibermax polycrystalline mullite fibers to produce a product that is high-temperaure (1650°C / 3000°F) resistant and virtually shot-free.Fibermax Mat contains no organic binders or other additives which cause outgassing fumes or associated problems. In addition to exhibiting excellent resistance to attack from most corrosive agents (exceptions include hydrofluoric acid, phosphoric acid and strong alkalies), Fibermax fiber also resists oxidation and reduction.Typical ApplicationsExpansion joint packingBurner wrapsBatten strips with fiber modulesAluminum homogenizing furnace liningsInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Specific Gravity 3.00 g/cc
3.00 g/cc
Density 0.0240 g/cc
0.000868 lb/in³
Thermal Properties Metric English Comments
Specific Heat Capacity 1.246 J/g-°C

@Temperature 1093 °C
0.2978 BTU/lb-°F

@Temperature 1999 °F
Melting Point 1870 °C
3400 °F
Maximum Service Temperature, Air 1566 °C
2851 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 72 %
72 %
CaO 0.050 %
0.050 %
Fe2O3 0.020 %
0.020 %
MgO 0.050 %
0.050 %
SiO2 27 %
27 %
TiO2 0.0010 %
0.0010 %
Descriptive Properties Value Comments
Color White
Fiber Diameter (microns) 2-3.5
Fiber Surface Area (m2/g) 7.65
Leachable Chlorides (ppm) 11
Na2O3 (%) 0.1
Temperature Grade (°C) 1650