Unipetrol Liquid Sulfur

Category Fluid , Solvent
Manufacturer Unipetrol RPA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol Liquid Sulfur.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Liquid sulphur is a viscous liquid of yellowish brown colour. It is produced by burning of hydrogen sulphide at the Claus Units. Liquid sulphur is used in sulphuric acid production and for other technical purposes.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Ash <= 0.050 %
<= 0.050 %
Component Elements Properties Metric English Comments
Sulfur, S 99.8 %
99.8 %
Chemical Properties Metric English Comments
Total Acid Number <= 0.050
<= 0.050
acidity
Descriptive Properties Value Comments
Organic Materials (bitumen) %, max 0.1