Nano composite nylonInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50% RH
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.20 mm
0.0080 in/in

@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 72.0 MPa
10400 psi
ASTM D790
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 2.11 J/cm
3.95 ft-lb/in
ASTM D256