Material Notes:
Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and others, and extruding the composite resins into plates, and laminating and heat-pressing the plates. UNILATE plates and boards are superior in heat resistance, withstand voltage, strength, and processability to the plates and boards of thermoplastic resins such as nylon, polyacetal, and others. The UNILATE plates and boards are greatly improved in water-absorbing property, electrical properties, and processability, compared to other thermosetting resin laminated sheets used in electric insulation applications.Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 56.0 MPa
8120 psi
Horizontal; ASTM D570
95.0 MPa
13800 psi
Vertical; ASTM D570
Elongation at Break 2.3 %
2.3 %
Horizontal; ASTM D570
2.6 %
2.6 %
Vertical; ASTM D570
Flexural Strength 120 MPa
17400 psi
Horizontal; ASTM D790
205 MPa
29700 psi
Vertical; ASTM D790
Flexural Modulus 5.50 GPa
798 ksi
Horizontal; ASTM D790
9.50 GPa
1380 ksi
Vertical; ASTM D790
Izod Impact, Unnotched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 46.0 µm/m-°C

@Temperature 25.0 - 100 °C
25.6 µin/in-°F

@Temperature 77.0 - 212 °F
Vertical; ASTM D696
106 µm/m-°C

@Temperature 25.0 - 100 °C
58.9 µin/in-°F

@Temperature 77.0 - 212 °F
Horizontal; ASTM D696
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 - 1.00e+13 ohm-cm
1.00e+10 - 1.00e+13 ohm-cm
ASTM D257
Surface Resistance 1.00e+10 - 1.00e+13 ohm
1.00e+10 - 1.00e+13 ohm
ASTM D257
Insulation Resistance 2.30e+14 ohm
2.30e+14 ohm
ASTM D257
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 35.0 kV/mm
889 kV/in
Under ambient atmosphere; ASTM D149
35.0 kV/mm
889 kV/in
After water absorption; ASTM D149
Arc Resistance 83 sec
83 sec
Comparative Tracking Index 200 V
200 V
IEC 112
Descriptive Properties Value Comments
Appearance Opaque