Universal Wire Works 502 (AMS 6466) Low Alloy Steel Welding Wire

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 502 (AMS 6466) Low Alloy Steel Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 502 is a 5% chromium, 0.5% molybdenum alloy for use as filler metal for welding low-alloy steels where response to heat treatment is required in weld. Used extensively with the gas metal arc, gas tungsten arc and submerged arc welding processes.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 5.5 %
5.5 %
Copper, Cu <= 0.35 %
<= 0.35 %
Iron, Fe 93.5 %
93.5 %
As Remainder
Manganese, Mn <= 0.60 %
<= 0.60 %
Molybdenum, Mo 0.50 %
0.50 %
Nickel, Ni <= 0.60 %
<= 0.60 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S <= 0.030 %
<= 0.030 %