Universal Wire Works BAg-2 (AMS 4768) Silver Brazing Filler Metal

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works BAg-2 (AMS 4768) Silver Brazing Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Thermal Properties Metric English Comments
Melting Point 607.2 - 701.7 °C
1125 - 1295 °F
Solidus 607.2 °C
1125 °F
Liquidus 701.7 °C
1295 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 18 %
18 %
Copper, Cu 26 %
26 %
Silver, Ag 35 %
35 %
Zinc, Zn 21 %
21 %