Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vicone High Performance Rubber VicoSil™ 139DLK-BL High Performance Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Vicone High Performance Rubber
Trade Name VicoSil™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSil™ 139DLK-BL High Performance Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FDA Approved
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ASTM D2240
Tensile Strength 7.20 MPa
1040 psi
ASTM D412
Elongation at Break 545 %
545 %
ASTM D412
Compressive Modulus 0.00180 GPa

@Strain 5 %
0.261 ksi

@Strain 5 %
ISO-7743
0.00190 GPa

@Strain 10 %
0.276 ksi

@Strain 10 %
ISO-7743
0.00220 GPa

@Strain 20 %
0.319 ksi

@Strain 20 %
ISO-7743
0.00260 GPa

@Strain 25 %
0.377 ksi

@Strain 25 %
ISO-7743
Compression Set 20 %
20 %
ASTM D395
Tensile Set 6.0 %
6.0 %
ASTM D412
Descriptive Properties Value Comments
Color Blue
Effect of Liquids - Change in Elongation (%) -12.1
ASTM D471
Effect of Liquids - Change in Hardness (%) -5
ASTM D471
Effect of Liquids - Change in Tensile Strength (%) -6.3
ASTM D471
Effect of Liquids - Change in Volume after Oil Immersion (%) 7.7
ASTM D471
Heat Aging - Change in Elongation (%) -36
ASTM D573
Heat Aging - Change in Hardness (%) 6
ASTM D573; 200°C; 72h
Heat Aging - Change in Tensile Strength (%) -21.42
ASTM D573