Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film

Category Polymer , Film , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name APTIV®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications offering an alternative option to the APTIV 1000 natural product.APTIV 1300 film has a unique combination of properties providing high temperature performance, light weight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products and low moisture absorption in a film format. Inherently halogen free and providing ease of processing makes APTIV films a technology enabler.Applications:Acoustic speaker diaphragms and voice coilsCompositesAerospace insulationPressure sensitive tapesWashers in high speed motorsWashers in mobile phone hingesFlexible surface heatersPressure sensor membranesProven temperature resistance to use of lead free soldersFeaturesHigh heat resistanceExcellent tribiological propertiesBroad chemical resistanceLow moisture absorptionHigh strength and toughnessStable, excellent electrical insulation propertiesGood flammability performance without use of flame retardant additivesInherently halogen freeRadiation resistanceLow smoke and toxic gas emissionExcellent hydrolysis resistanceExcellent acoustic propertiesHigh purityLight weightRecyclableEasy to process - can be laminated to other materials, thermoformed, metallized, coated, printed, stamped and die cut, welded, heat sealed, and coated.Information Provided by VICTREX®
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc

@Temperature 23.0 °C
1.30 g/cc

@Temperature 73.4 °F
ISO 1183
Thickness 50.0 microns
1.97 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD >= 150 %
>= 150 %
ISO 527
Film Elongation at Break, TD >= 150 %
>= 150 %
ISO 527
Tensile Modulus 2.30 GPa
334 ksi
TD; ISO 527
2.40 GPa
348 ksi
MD; ISO 527
Film Tensile Strength at Break, MD 120 MPa
17400 psi
ISO 527
Film Tensile Strength at Break, TD 110 MPa
16000 psi
ISO 527
Thermal Properties Metric English Comments
Shrinkage, MD <= 2.0 %

@Temperature 200 °C
<= 2.0 %

@Temperature 392 °F
TM-VX-84
<= 2.0 %

@Temperature 200 °C
<= 2.0 %

@Temperature 392 °F
TM-VX-84
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+16 ohm-cm

@Temperature 23.0 °C
4.00e+16 ohm-cm

@Temperature 73.4 °F
100V; ASTM D257
Dielectric Strength 190 kV/mm
4830 kV/in
MD, 6.25mm (0.25in) electrode; ASTM D149
190 kV/mm
4830 kV/in
TD, 6.25mm (0.25in) electrode; ASTM D149
Users viewing this material also viewed the following: