Material Notes:
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for composite manufacture, easy flow, FDA food contact compliantInformation provided by Victrex
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
ISO 1183
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Particle Size 10 µm
10 µm
D<sub>50</sub>; ISO 13320-1
Viscosity 130000 cP

@Temperature 400 °C
130000 cP

@Temperature 752 °F
Melt; ISO 11443
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
Result based on similar products; ISO 527
Elongation at Break 15 %
15 %
Result based on similar products; ISO 527
Tensile Modulus 4.10 GPa
595 ksi
Result based on similar products; ISO 527
Flexural Strength 170 MPa
24700 psi
Result based on similar products; ISO 178
Flexural Modulus 3.90 GPa
566 ksi
Result based on similar products; ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
Result based on similar products; ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
Result based on similar products; ISO 180/U
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
ISO 11357
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
147 °C
297 °F
Midpoint; ISO 11357
Processing Properties Metric English Comments
Processing Temperature 380 - 400 °C
716 - 752 °F
Dry Time 3 hour

@Temperature 150 °C
3 hour

@Temperature 302 °F
5 hour

@Temperature 120 °C
5 hour

@Temperature 248 °F
Descriptive Properties Value Comments
Color Natural