Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® PEEK 150XF Polyetheretherketone, Unreinforced

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Victrex
Trade Name PEEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® PEEK 150XF Polyetheretherketone, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, colour natural.Information Provided by VICTREX®
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
ISO 1183
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Particle Size 25 µm
25 µm
D<sub>50</sub>; ISO 13320-1
Viscosity 130000 cP
130000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa

@Temperature 23.0 °C
14500 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 15 %

@Temperature 23.0 °C
15 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 4.10 GPa

@Temperature 23.0 °C
595 ksi

@Temperature 73.4 °F
ISO 527
Flexural Strength 170 MPa

@Temperature 23.0 °C
24700 psi

@Temperature 73.4 °F
ISO 178
Flexural Modulus 3.90 GPa

@Temperature 23.0 °C
566 ksi

@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/U
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
ISO 11357
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
147 °C
297 °F
Midpoint; ISO 11357
Processing Properties Metric English Comments
Processing Temperature 380 - 400 °C
716 - 752 °F
Drying Temperature 120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Copyright © lookpolymers.com All Rights Reserved