Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® 705 Black Polyetheretherketone (PEEK) Powder Coating

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® Vicote® 705 Black Polyetheretherketone (PEEK) Powder Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VICOTE 705Blk is a black pigmented version of the 705 grade. This grade has a nominal particle size of about 50 microns. The powder is dark grey in colour and is a low melt viscosity grade for lower film builds. Typical film thicknesses range from 50 - 80 microns. The final coating takes on a dark gun metal grey colour after stoving.VICOTE Coatings, like other noncoating grades of VICTREX PEEK polymer, are thermoplastic in nature and exhibit flow above the melt temperature. When processed using the correct guidelines the coatings will exhibit the excellent properties that VICTREX PEEK polymer is renowned for.Typical properties are high continuous use temperature of 260°C, excellent wear, abrasion and cut through resistance at these high temperatures combined with excellent chemical and radiation resistance. VICOTE Coatings have a low level of extractables and are hydrolysis resistant and inherently flame retardant. Meets FDA 21 CFR 175.300Information Provided by VICTREX®
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Glass Transition Temp, Tg 143 °C
289 °F
DSC
UL RTI, Electrical 260 °C
500 °F
UL 746B
Descriptive Properties Value Comments
Konig Hardness (seconds) 200
Test Method: BS EN ISO 1522