Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® F814 Polyetheretherketone (PEEK) Liquid Dispersion

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® Vicote® F814 Polyetheretherketone (PEEK) Liquid Dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VICOTE F814 has been specifically formulated to provide a resilient coating with high wear and abrasion resistance on ferrous and non-ferrous metals such as carbon and cast steel. These properties are retained at high temperatures where other coatings would potentially fail. Typical properties are high continuous use temperature of 280°C, excellent wear, abrasion and cut through resistance at these high temperatures combined with excellent chemical resistance. VICOTE dispersions have a low level of extractables and are inherently flame retardant.All information provided by Victrex.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ISO 2811
Solids Content 28.1 %
28.1 %
Theory Volume
37.4 %
37.4 %
weight; Internal Test
pH 10
10
Viscosity Measurement 60

@Temperature 25.0 °C
60

@Temperature 77.0 °F
BSEN ISO 2431
Mechanical Properties Metric English Comments
Impact 1.0
1.0
1m, 2kg, Indent 5mm; ISO 6272
Coefficient of Friction 0.54
0.54
µm @ 10 min., Using 250N Load; ASTM G 133
Thermal Properties Metric English Comments
Melting Point 372 °C
702 °F
DSC
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Color Off White
Konig Hardness (seconds) 142
ISO 1522