Voloknohim PA-TM15 Glass and Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Voloknohim
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Voloknohim PA-TM15 Glass and Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Voloknokhim
Physical Properties Metric English Comments
Filler Content 12 - 18 %
12 - 18 %
Particle Size 2000 - 5000 µm
2000 - 5000 µm
at least 97%
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Mechanical Properties Metric English Comments
Elongation at Break >= 6.0 %
>= 6.0 %
Modulus of Elasticity 4.00 GPa
580 ksi
When curved
Transverse Strength >= 90.0 MPa
>= 13100 psi
when destroyed
Tear Strength Test >= 68
>= 68
MPa