Category | Polymer , Thermoset , Filled/Reinforced Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Elastomer, for Thermal Management |
Manufacturer | Von Roll Isola |
Trade Name | IMI Transtherm® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Von Roll Isola IMI Transtherm® T 1500-10 Silicone Elastomer, Fiberglass Reinforced, Boron Nitride Filled, for Thermal Management.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.50 g/cc | 0.0542 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 80 | 80 | ASTM D2240 |
Tensile Strength, Ultimate | 45.0 MPa | 6530 psi | ASTM D828 |
Elongation at Break | 2.0 - 4.0 % | 2.0 - 4.0 % | ASTM D828 |
Tear Strength Test | 120 | 120 | lb (force) Cut-Through Resistance; IMI Test |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | typical TO-3 test value per MIL-I-49546A |
Maximum Service Temperature, Air | 180 °C | 356 °F | Continuous use temperature per MIL-I-49546A |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
Dielectric Constant | 2.47 @Frequency 1e+6 Hz |
2.47 @Frequency 1e+6 Hz |
ASTM D150 |
2.56 @Frequency 60 Hz |
2.56 @Frequency 60 Hz |
ASTM D150 | |
Dielectric Strength | 16.0 kV/mm | 406 kV/in | Dry, ASTM D149 |
Dissipation Factor | 0.00060 @Frequency 1000 Hz |
0.00060 @Frequency 1000 Hz |
ASTM D150 |
0.00070 @Frequency 60 Hz |
0.00070 @Frequency 60 Hz |
ASTM D150 |