Von Roll Isola IMI Varnish 73538 Solventless Polyester Varnish for Electrical Insulation

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Solventless Electrical Varnish
Manufacturer Von Roll Isola
Trade Name IMI Varnish
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Von Roll Isola IMI Varnish 73538 Solventless Polyester Varnish for Electrical Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 30°C. Usage Notes: Trickle resin for small, high-speed armatures.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Viscosity 250 cP
250 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Electrical Properties Metric English Comments
Dielectric Strength 12.0 kV/mm
305 kV/in
Processing Properties Metric English Comments
Processing Temperature 155 °C
311 °F
Suggested baking time at this temperature is 0.5-1 hr.