Von Roll Isola IMI Varnish 9522 Polyester Varnish for Electrical Insulation

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Solventless Electrical Varnish
Manufacturer Von Roll Isola
Trade Name IMI Varnish
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Von Roll Isola IMI Varnish 9522 Polyester Varnish for Electrical Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Von Roll Isola USA.Flash Point: 24°C. Average solids: 50%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, bare copper coils, etc. where good adhesion is desired.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Viscosity 205 cP
205 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
Electrical Properties Metric English Comments
Dielectric Strength 114 kV/mm
2900 kV/in
Processing Properties Metric English Comments
Processing Temperature 150 °C
302 °F
Suggested baking time at this temperature is 4-6 hr.