Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound

Category Polymer , Thermoset , Epoxy , Epoxy Molding Compound , Filled/Reinforced Thermoset
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name Neopreg Kinel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Long aramid fiber reinforced BMI molding compound suited for very demanding tribologic applications under medium to poor lubricated conditions, high temperatures & PV levelsInformation provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ISO 60
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Water Absorption 0.60 %
0.60 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-1
Elongation at Break 0.60 %
0.60 %
ISO 527-1
Tensile Modulus 16.0 GPa
2320 ksi
ISO 527-1
Flexural Strength 136 MPa
19700 psi
ISO 178
Flexural Modulus 11.0 GPa
1600 ksi
ISO 178
Compressive Strength 132 MPa
19100 psi
ISO 604
Charpy Impact, Notched 2.40 J/cm²
11.4 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 275 °C
527 °F
Descriptive Properties Value Comments
Color Dark Grey
Molding Method Compression
Injection
Transfer