Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-1180H Super Hard Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1180H Super Hard Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low mold shrinkage, good impact resistance, perfect transparency, good mold release, fatigue resistance, chemical & hydrolytic resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength 46.0 MPa
6670 psi
ASTM D412
Elongation at Break 430 %
430 %
ASTM D412
100% Modulus 0.0330 GPa
4.79 ksi
ASTM D412
300% Modulus 0.0380 GPa
5.51 ksi
ASTM D412
Tear Strength 240 kN/m
1370 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 190 - 220 °C
374 - 428 °F
Users viewing this material also viewed the following: