Wanhua Chemical Wanthane® WHT-1195 Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1195 Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength 39.0 MPa
5660 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
100% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
300% Modulus 0.0290 GPa
4.21 ksi
ASTM D412
Tear Strength 120 kN/m
685 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 195 - 215 °C
383 - 419 °F