Wanhua Chemical Wanthane® WHT-1565 Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1565 Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
ASTM D2240
Tensile Strength 25.0 MPa
3630 psi
ASTM D412
Elongation at Break 750 %
750 %
ASTM D412
100% Modulus 0.00300 GPa
0.435 ksi
ASTM D412
300% Modulus 0.00600 GPa
0.870 ksi
ASTM D412
Tear Strength 70.0 kN/m
399 pli
ASTM D624
Abrasion 50
50
Abrasion resistance, mm<sup>3</sup>; ISO 4649
Processing Properties Metric English Comments
Processing Temperature 170 - 190 °C
338 - 374 °F