Wanhua Chemical Wanthane® WHT-2185 Polycaprolactone Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-2185 Polycaprolactone Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 26.0 MPa
3770 psi
ASTM D412
Elongation at Break 520 %
520 %
ASTM D412
100% Modulus 0.00600 GPa
0.870 ksi
ASTM D412
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
Tear Strength 110 kN/m
628 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 185 - 205 °C
365 - 401 °F
Users viewing this material also viewed the following: