Wanhua Chemical Wanthane® WHT-7190 Polycaprolactone Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-7190 Polycaprolactone Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength 40.0 MPa
5800 psi
ASTM D412
Elongation at Break 330 %
330 %
ASTM D412
100% Modulus 0.0100 GPa
1.45 ksi
ASTM D412
300% Modulus 0.0350 GPa
5.08 ksi
ASTM D412
Tear Strength 110 kN/m
628 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 195 - 215 °C
383 - 419 °F