Wanhua Chemical Wanthane® WHT-8195 Polyether-Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-8195 Polyether-Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength 30.0 MPa
4350 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
100% Modulus 0.0130 GPa
1.89 ksi
ASTM D412
300% Modulus 0.0280 GPa
4.06 ksi
ASTM D412
Tear Strength 110 kN/m
628 pli
ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F