Washington Penn H2GF3 Polypropylene, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Washington Penn
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn H2GF3 Polypropylene, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer. Excellent heat aged physical properties.Applications: Under hood applications, battery trays, exercise equipmentData provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min
5.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 76.0 MPa
11000 psi
ASTM D638
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
Flexural Modulus 5.00 GPa
725 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.900 J/cm

@Thickness 3.17 mm
1.69 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm

@Thickness 3.17 mm
5.99 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 144 °C
291 °F
ASTM D648