Weartech International NOREM 02A Iron Hardfacing & Wear Resistant Alloy

Category Metal , Ferrous Metal
Manufacturer Weartech
Trade Name NOREM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Weartech International NOREM 02A Iron Hardfacing & Wear Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: for cobalt-free components in nuclear applications, valvesInformation provided by Weartech International, Norem is a registered trademark of Electric Power Research Institute
Mechanical Properties Metric English Comments
Hardness, Rockwell C 36 - 42
36 - 42
Component Elements Properties Metric English Comments
Carbon, C 1.25 %
1.25 %
Chromium, Cr 25 %
25 %
Iron, Fe 59.89 %
59.89 %
Manganese, Mn 4.5 %
4.5 %
Molybdenum, Mo 2.0 %
2.0 %
Nickel, Ni 4.0 %
4.0 %
Nitrogen, N <= 0.060 %
<= 0.060 %
Silicon, Si 3.3 %
3.3 %
Descriptive Properties Value Comments
Relative Wear Performance Cold Abrasion
Good/Moderate
Corrosion
Not Recommended
Erosion
Excellent
Hot Abrasion
Not Recommended
Impact
Not Recommended
Metal to Metal
Excellent