Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® FR1841-N1 Nylon 66, Unfilled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527-93
Elongation at Break 5.0 %
5.0 %
ISO 527-93
Flexural Strength 100 MPa
14500 psi
ISO 178-93
Flexural Modulus 3.20 GPa
464 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-93
Flammability, UL94 V-0

@Thickness 0.790 mm
V-0

@Thickness 0.0311 in