Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GF1750-BK2 50% Glass Fiber Reinforced Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF1750-BK2 50% Glass Fiber Reinforced Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183-87
Filler Content 50 %
50 %
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
ISO 527-93
Elongation at Break 1.7 %
1.7 %
ISO 527-93
Flexural Strength 255 MPa
37000 psi
ISO 178-93
Flexural Modulus 14.8 GPa
2150 ksi
ISO 178-93
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-93
Users viewing this material also viewed the following: