Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GF25-66 XE-NBK1 25% Glass Fiber Reinforced, Engineering Grade Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Carbon Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF25-66 XE-NBK1 25% Glass Fiber Reinforced, Engineering Grade Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183-87
Filler Content 25 %
25 %
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ISO DIS 294-5
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO 527-93
Elongation at Break 3.0 %
3.0 %
ISO 527-93
Flexural Strength 220 MPa
31900 psi
ISO 178-93
Flexural Modulus 7.50 GPa
1090 ksi
ISO 178-93
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ISO 75-93