Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 60% Glass Fiber Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ISO 1183-87
Filler Content 60 %
60 %
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 215 MPa
31200 psi
ISO 527-93
Elongation at Break 2.2 %
2.2 %
ISO 527-93
Flexural Strength 325 MPa
47100 psi
ISO 178-93
Flexural Modulus 17.8 GPa
2580 ksi
ISO 178-93
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ISO 75-93