Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® MR409 22H-NBK1 Nylon 66, 40% Mineral Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MR409 22H-NBK1 Nylon 66, 40% Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm
0.012 - 0.016 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-93
Elongation at Break 6.0 %
6.0 %
ISO 527-93
Flexural Strength 125 MPa
18100 psi
ISO 178-93
Flexural Modulus 5.70 GPa
827 ksi
ISO 178-93
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO 75-93
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved