Wellman Wellamid® MRGF25/15 22H-NBK1 40% Mineral/Glass Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGF25/15 22H-NBK1 40% Mineral/Glass Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mineral/Glass Reinforced Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183-87
Filler Content 40 %
40 %
Linear Mold Shrinkage, Flow 0.0025 - 0.0055 cm/cm
0.0025 - 0.0055 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527-93
Elongation at Break 3.0 %
3.0 %
ISO 527-93
Flexural Strength 165 MPa
23900 psi
ISO 178-93
Flexural Modulus 8.85 GPa
1280 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.20 kJ/m²
2.00 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ISO 75-93