Wellman Wellamid® MRGF25/15 42H-BK167A Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGF25/15 42H-BK167A Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GM 167A Black color matchAll information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527-93
Elongation at Break 2.0 %
2.0 %
ISO 527-93
Flexural Strength 170 MPa
24700 psi
ISO 178-93
Flexural Modulus 10.1 GPa
1460 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-93