Wellman Wellamid® MRGST1715-WBK1 Nylon 6, 25% Mineral and Glass Sphere Reinforced, Impact Modified, Weatherable Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGST1715-WBK1 Nylon 6, 25% Mineral and Glass Sphere Reinforced, Impact Modified, Weatherable Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527-93
Elongation at Break 7.0 %
7.0 %
ISO 527-93
Flexural Strength 95.0 MPa
13800 psi
ISO 178-93
Flexural Modulus 4.50 GPa
653 ksi
ISO 178-93
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-93