Wellman Wellamid® MRT1487 N Nylon 66, 32% Mineral Reinforced, Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Mineral Filled, Impact Grade
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRT1487 N Nylon 66, 32% Mineral Reinforced, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527-93
Elongation at Break 15 %
15 %
ISO 527-93
Flexural Strength 100 MPa
14500 psi
ISO 178-93
Flexural Modulus 3.60 GPa
522 ksi
ISO 178-93
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75-93