Westlake EBAC® Plus SP1903 18% Ethylene Butyl Acrylate Copolymer

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Westlake Chemical Corporation
Trade Name EBAC® Plus
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EBAC® Plus SP1903 18% Ethylene Butyl Acrylate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake EBAC® SP1903 is an 18% EBA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1903 provides excellent adhesion to polyolefins, polyesters, and other polymers while providing outstanding low temperature performance.Applications: films, disposable gloves and wound care.FDA: This material complies with FDA regulations in 21 CFR, section 177.1340.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Butyl Acrylate Content 18 %
18 %
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ASTM D2240
Tensile Strength at Break 14.0 MPa
2030 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 730 %
730 %
500mm/min; ASTM D638 Type IV Specimen
Thermal Properties Metric English Comments
Melting Point 102 °C
216 °F
by DSC; ASTM D3418
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Blown Film
Extrusion
Film
Region US & Canada
Bamberger Polymers Distribution