Material Notes:
Westlake EBAC® SP1802 is a 22.5% EBA copolymer designed for blown film, tie-layer, coextrusions and blending where flexibility and strength are important. SP1802 provides excellent elasticity and low temperature performance.Applications: films, flexible packaging, disposable gloves, IV containers and wound care.FDA: This material complies with FDA regulations in 21 CFR, section 177.1340.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ASTM D1505
Butyl Acrylate Content 22.5 %
22.5 %
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ASTM D2240
Tensile Strength at Break 13.0 MPa
1890 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 848 %
848 %
500mm/min; ASTM D638 Type IV Specimen
Thermal Properties Metric English Comments
Melting Point 86.0 °C
187 °F
by DSC; ASTM D3418
Vicat Softening Point 59.0 °C
138 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Blown Film
Extrusion
Film
Region US & Canada
Bamberger Polymers Distribution