Material Notes:
WESTLAKE low-density polyethylene EC4042 is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seals at high packaging or sealing rates.Application/UsesFood packagingFreezer wrapFrozen food packagingSugar pouchesFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.00 MPa
1310 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 300 %
300 %
500mm/min; ASTM D638 Type IV Specimen
2% Secant Modulus 0.235 GPa
34.1 ksi
12.7mm/min; ASTM D790
Processing Properties Metric English Comments
Melt Temperature 149 - 166 °C
300 - 330 °F
Descriptive Properties Value Comments
Process Coating
Region US & Canada
Bamberger Polymers Distribution