Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Coating Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to 600°F, Non-Corrosive at Extrusion Temperatures, FDA Clearance for Packaging of Most Foods - including Aseptic Packaging, No FDA thickness limitationApplications:Coatings & Laminations: Higher Neck-In but Similar Drawdown vs. LDPE Extrusion Coating Grades, Excellent Heat Seal Response at Low Seal Temperatures, Adheres Very Well to Non-Porous Substrates such as OPP, PVDC Coated Substrates, and Polyester, Adheres well to Porous Substrates such as Paper and Paperboard; Compounding: Impact Modification, Compatibilizer; Film: Tie Layers for LDPE, LLDPE, HDPE, PET, PP, PVDC, Ionomer, EVA, EAA, PVC (Rigid), PCEastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ASTM D1505
ESCR 10% Igepal® >= 360 hour

@Temperature 50.0 °C
>= 360 hour

@Temperature 122 °F
F<sub>50</sub>; ASTM D1693
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Cond. E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
ASTM D2240
Hardness, Shore D 33
33
ASTM D2240
Tensile Strength, Ultimate 12.0 MPa
1740 psi
ASTM D638
Elongation at Break 780 %
780 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 83.0 °C
181 °F
by DSC
Vicat Softening Point 59.0 °C
138 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 154 °C
309 °F
Blown Film
190 °C
374 °F
Molding
315 °C
599 °F
Extrusion Coating