Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Elevate™ EF545 4% Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Westlake Chemical Corporation
Trade Name Elevate™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Elevate™ EF545 4% Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake EF545 resin is a 4% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low temperature brittleness properties.Application/UsesHigh clarity packagingLight and medium duty produce bagsLinear blend component for sealing and clarityFDA: This material complies with FDA regulations in 21 CFR, section 177.1350. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Vinyl Acetate Content 4.0 %
4.0 %
Thickness 31.8 microns
1.25 mil
Melt Flow 0.55 g/10 min
0.55 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 225 %
225 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Dart Drop Test 160 g
0.353 lb
ASTM D1709
Film Tensile Strength at Break, MD 22.8 MPa
3300 psi
ASTM D882
Film Tensile Strength at Break, TD 17.9 MPa
2600 psi
ASTM D882
1% Secant Modulus, MD 172 MPa
25000 psi
ASTM D882
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 13 %
13 %
ASTM D1003
Gloss 50 %
50 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved