Westlake LF1020 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant product is available with various slip and antiblock formulations.Application/UsesStretch wrapAgricultural filmsTrash bagsCo-extruded structuresFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 1.1 g/10 min
1.1 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.3 MPa
1500 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa
1500 psi
ASTM D882
Dart Drop 4.72 g/micron
120 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 35.9 MPa
5200 psi
ASTM D882
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 204 - 216 °C
400 - 420 °F
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film