Material Notes:
Mxsten CV plastomer CV77529 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this resin exhibit very good strength properties and low seal initiation temperatures.Application/UsesAgricultural tubingBlown filmCo-ex filmsFDA: This material complies with FDA regulations in 21 CFR, section 177.1520.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.906 g/cc
0.0327 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 6.89 MPa
1000 psi
ASTM D882
Film Elongation at Break, MD 550 %
550 %
ASTM D882
Film Elongation at Break, TD 950 %
950 %
ASTM D882
Elmendorf Tear Strength MD 440 g
440 g
ASTM D1922
Elmendorf Tear Strength TD 600 g
600 g
ASTM D1922
Dart Drop 63.0 g/micron
1600 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 66.2 MPa
9600 psi
ASTM D882
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
1% Secant Modulus, TD 138 MPa
20000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 14 %
14 %
ASTM D1003
Gloss 60 %
60 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Blow-up Ratio (BUR) 2.4
2.4
Descriptive Properties Value Comments
Process Blown Film