Material Notes:
HTP 800 is a clear PVC based material for use as windows and doors in cleanroom equipment. Notable properties include light transmission, chemical resistance, and flame resistance. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Water Absorption 0.016 %
0.016 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D785
Tensile Strength, Yield 60.06 MPa
8711 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Flexural Strength 96.87 MPa
14050 psi
ASTM D790
Flexural Modulus 3.0030 GPa
435.55 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 - 95.0 °C
194 - 203 °F
Continuous Use
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648
Flammability, UL94 V-0
V-0
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
ASTM D149; at 1 mil