Material Notes:
Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impact strength, and a broad service use temperature. This polymer offers extremely low permeability to liquids, gases, and vapors.Halar® is a trade name of Solvay Solexis, Inc. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.6 MPa
4300 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Tensile Modulus 1.65 GPa
240 ksi
ASTM D638
Flexural Yield Strength 26.2 MPa
3800 psi
ASTM D790
Flexural Modulus 1.69 GPa
245 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 101 µm/m-°C

@Temperature 20.0 °C
56.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 241 °C
465 °F
ASTM D4591
Maximum Service Temperature, Air 149 °C
300 °F
Continuous Use
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
ASTM D648
Flammability, UL94 V-0
V-0
Oxygen Index 56 %
56 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 1000 Hz
2.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 13.8 kV/mm
350 kV/in
ASTM D149