Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Westlake Plastics
Trade Name KYNAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-sloughing carbon-fiber-filled material with resistance to most chemicals and solvents mechanically strong and tough, thermally stable to 335F, flame and abrasion resistant, and easily fabricated into finished parts. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
ASTM D2240
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 183 MPa
26500 psi
ASTM D790
Flexural Modulus 8.55 GPa
1240 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 168 °C
335 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Dry; ASTM D257
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Dry; ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
15% RH; MIL-B-81705-B