Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Lennite® SD-P UHMW-PE (static dissipative)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Westlake Plastics
Trade Name Lennite® SD-P
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Lennite® SD-P UHMW-PE (static dissipative).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon-powder filled, self-lubricating, moisture-repellent material with resistivity levels in the 10^5-10^9 range. This material has the highest impact strength, is lightweight, has excellent abrasion resistance, and possesses good chemical and stress-crack resistance. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 21.6 MPa
3130 psi
ASTM D638
Elongation at Break 310 %
310 %
ASTM D638
Flexural Modulus 1.05 GPa
152 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 78.9 °C
174 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.1 °C
115 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+7 ohm-cm
1.90e+7 ohm-cm
Dry; ASTM D257
Surface Resistance 1.20e+7 ohm
1.20e+7 ohm
Dry; ASTM D257