Westlake Plastics Propylux® SD-A Polypropylene (anti-static)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Westlake Plastics
Trade Name Propylux® SD-A
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Propylux® SD-A Polypropylene (anti-static).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-carbon-filled, permanently static-dissipative material, with good chemical resistance and mechanical properties. This material is light weight, weldable, easily machined and fabricated, available in natural or black color, and has moderate transparency at thinner gauges. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Water Absorption 1.0 %
1.0 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength, Yield 30.3 MPa
4400 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Strength 42.7 MPa
6200 psi
ASTM D790
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
227 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C
135 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 - 1.00e+11 ohm-cm
1.00e+9 - 1.00e+11 ohm-cm
Dry; ASTM D257
Surface Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
Dry; ASTM D257
Static Decay <= 0.30 sec
<= 0.30 sec
15% RH; MIL-B-81705-B