Material Notes:
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad chemical resistance. Tempalux stock shapes are inherently flame resistant with low smoke emission. Tempalux stock shapes display property retention and resistance to environmental stress cracking when exposed to a wide variety of chemicals. The standard color of Tempalux stock shapes is light amber. Glass filled grades appear tan or greenish in color. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.19 %
0.19 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Rockwell M 114
114
ASTM D7852
Tensile Strength at Break 139 MPa
20100 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 6.89 GPa
1000 ksi
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Compressive Yield Strength 198 MPa
28700 psi
ASTM D695
Compressive Modulus 5.58 GPa
809 ksi
ASTM D695
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.81 J/cm
9.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.245 W/m-K
1.70 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
408 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.406 mm
V-0

@Thickness 0.0160 in
Oxygen Index 50 %
50 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 26.4 kV/mm
670 kV/in
ASTM D149
Dissipation Factor 0.0025

@Frequency 1000 Hz
0.0025

@Frequency 1000 Hz
ASTM D150