Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 40% Glass Filled
Manufacturer Westlake Plastics
Trade Name Zelux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and impact strength are essential including lenses, manifolds, site glasses and machine guards. Zelux is used for a wide range of electrical applications since it has low moisture absorption and good insulating properties. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Water Absorption 0.12 %
0.12 %
ASTM D570; 24 hrs.
Water Absorption at Saturation 0.23 %
0.23 %
ASTM D570; at equilibrium
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93
93
ASTM D7852
Tensile Strength, Yield 159 MPa
23000 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 11.6 GPa
1680 ksi
ASTM D638
Flexural Yield Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
ASTM D790
Compressive Strength 145 MPa
21000 psi
ASTM D695
Compressive Modulus 10.3 GPa
1500 ksi
ASTM D695
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 °C
9.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.12 mm
V-1

@Thickness 0.0440 in
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.53

@Frequency 60 Hz
3.53

@Frequency 60 Hz
ASTM D150
Dielectric Strength 45.0 kV/mm
1140 kV/in
ASTM D149
Dissipation Factor 0.0013

@Frequency 60 Hz
0.0013

@Frequency 60 Hz
ASTM D150
Users viewing this material also viewed the following: