Wico Plast Wicoran 37 ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Wico Plast
Trade Name Wicoran
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wico Plast Wicoran 37 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH
Physical Properties Metric English Comments
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Izod Impact, Unnotched 2.15 J/cm
4.03 ft-lb/in
ASTM D256